Comparison of Micromechanical Parameters of Different Dental Implants Using Nanoindentation

The aim of this work is the description of microstructure and comparison of micromechanical properties of cylindrical shaped intraosseous parts of dental implants with plasma modified surface and with threaded modification. Differences in elastic parameters (such as reduced modulus (Er) and hardness (H)) of investigated implants within the supporting part of the shaft and surface layer in two different directions (proximal and lateral) are compared using experimental method of nanoindentation.